| Sign In | Join Free | My qualitytoyschina.com |
|
| Categories | High Temperature Alloy |
|---|---|
| Brand Name: | KAIXIN |
| Model Number: | KX-Alloy605 |
| Certification: | ISO9001:2015 |
| Place of Origin: | China |
| MOQ: | 200KG |
| Price: | To negotiate |
| Payment Terms: | T/T, L/C |
| Supply Ability: | 50~80TONS per MONTH |
| Delivery Time: | 45~60days |
| Packaging Details: | Wooden Box, size as per guests request |
| Shape: | Wire, Strip, Rod, Tube, Plate |
| Alloy Type: | Nickel-based Deformed Superalloy |
| Raw Materials: | NI9-11%,CR19-21%,W14-16%,MO Rem |
| Executive Standard: | ASTM |
| Delivery State: | Sosoloid |
| Application: | Manufacture engine guide blade, turbine outer ring, outer wall, swirler, sealing plate and etc parts |
| Features: | Excellent stability and high strength |
| Size: | Negotiable |
| Company Info. |
| Danyang Kaixin Alloy Material Co., Ltd. |
| Verified Supplier |
| View Contact Details |
| Product List |
KX GH605 Light Rod Plate Structural Operating Temperature Range For High Temperature Alloy
Product Description and Application
GH605 is also known as L605,UNSR30605,GH5605
GH605 is a Co-Cr-Ni based solid solution enhanced deformation superalloy, its use temperature is below 1000℃. Cobalt-based superalloy GH605 is a cobalt base alloy strengthened by solution of 20%Cr and 15%W(percent mass). It has medium durability and creep strength below 815℃, excellent oxidation resistance below 1 090℃, and satisfactory process properties such as forming and welding. It is a key material for aero engine, rocket engine, naval ship and industrial gas turbine. Its development and production status is one of the symbols on the metal materials development level in a country. It is used for manufacturing the high temperature parts of aero engine guide blade, turbine outer ring, outer wall, swirler and sealing plate.
Process Performance and Requirements
Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)
| Composition | Fe | C | Si | Mn | P | S | Cr | Ni | W | More |
| Min | - | 0.05 | - | 1 | - | - | 19 | 9 | 14 | Co:Rem |
| Max | 3 | 0.15 | 0.4 | 2 | 0.04 | 0.03 | 21 | 11 | 16 |
| Density | p=9.13g/cm3 |
| Melting Temperature Range | 1330℃-1410℃ |
| Variety | Tensile Property in the Room Temperature | Hardness HV | 815℃ Durability | Grain Size/Grade | Other properties | ||||
| MPa | MPa | MPa | MPa | t/h | % | ||||
| Middle Plate,Sheet,Strip | ≧890 | 370-550 | ≧35 | ≤290 | 165 | ≧24 | ≧10 | ≧2.5(1) | Bend |
Cold Hard Strip Grade A | ≧1500 | ≧1300 | ≧5 | 410-480 | --- | ---- | --- | ≧9 | Bend |
Cold Hard Strip Grade B | ≧1700 | ≧1500 | ≧3 | 485-560 | --- | --- | --- | ≧10 | Bend |
| Bar | ≧860 | ≧340 | ≧35 | ≤ 282 | 165 | ≧ 23 | ≧10 | ≧2(0) | --- |
| Ring | ≧860 | ≧310 | ≧30 | ≤ 248 | 165 | ≧ 24 | ≧10 | ≧2(0) | --- |

Professional Customization
| Cold-drawn Wire | ¢0.3~¢18mm(Delivery in rolls or trays) |
| Hot-Rolling Wire | ¢5.5~¢20mm(Delivery in rolls) |
| Strip | thickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips) |
| Smooth Forged Rod on a Lathe | ¢60~350mm,L800-2500mm |
| Hot-rolled Burnishing | ¢20~80mm,L1000-5000mm |
| Cold Drawn and Burnishing | ¢2.5~18mm,L1000-8000mm |
| Seamless Tube | ¢1~275mm,wall thickness 0.2~30,L1000-8000mm |





|